Polymer Property : Viscosity = 6800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 5000 - 6800 cP
5000 - 6800 cP
Huntsman Araldite GY 6004 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 178 to 196. Max color is 1.Comments/Applications: Slightly modified GY 6010. Medium viscosity, general purpose, highly versatile resin for use in cold or heat-cured ..