Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7.35 - 2.50e+7 cP | 7.35 - 2.50e+7 cP | Average value: 151000 cP Grade Count:450 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Viscosity | 7.35 cP | 7.35 cP | ASTM-D562 |
Abatron Primkote 8006-1 All Purpose Epoxy Primer Primkote 8006-1 is an all purpose epoxy primer that excels as a primer for concrete, metal, and wood. It also performs well as a penetrating primer for weathered wood, concrete sealer, conditioner f.. |