Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
8.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
ASTM D3835 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer