Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 80.0 - 1450 cP | 80.0 - 1450 cP | Average value: 632 cP Grade Count:10 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |