Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Viscosity | 8800 cP @Shear Rate 11200 1/s, Temperature 200 °C |
8800 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Viscosity | 8800 cP @Temperature 175 °C |
8800 cP @Temperature 347 °F |
Shimadzu Viscosity, 1000 psi |
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min.. |
|||
Viscosity | 8800 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8800 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7170-1000 TPE Product Description: StarFlex P 7170-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Viscosity | 8800 cP | 8800 cP | |
Dymax 3072 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 8800 - 9800 cP @Temperature 35.0 °C |
8800 - 9800 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G120 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 8800 - 10200 cP @Temperature 35.0 °C |
8800 - 10200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G175 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |