Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200 - 880000 cP | 200 - 880000 cP | Average value: 48500 cP Grade Count:44 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |