Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9.0 cP @Temperature 0.000 °C |
9.0 cP @Temperature 32.0 °F |
|
Akzo Nobel Trigonox® 121 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates.Information provided by Akzo Nobel Polymer Chemicals. |