Physical Properties Metric English Comments
Grain Size 800 - 1000 µm
800 - 1000 µm
Sharadaa Ceramics Calcium Silicate Block
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..