Physical Properties Metric English Comments
Grain Size <= 8000 µm
<= 8000 µm
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..