Polymer Property : Apparent Bulk Density = 0.000542 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® LN 3000 Expandable Polystyrene
Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® LN 7000 Expandable Polystyrene
Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene  (discontinued **)
Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene  (discontinued **)
Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene  (discontinued **)
Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7..
Apparent Bulk Density 0.0150 g/cc
0.000542 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene  (discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..