Polymer Property : Apparent Bulk Density = 0.000686 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.0190 g/cc
0.000686 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® EH 3000 Expandable Polystyrene
Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u..
Apparent Bulk Density 0.0190 g/cc
0.000686 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene  (discontinued **)
Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200..
Apparent Bulk Density 0.0190 g/cc
0.000686 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene  (discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
Apparent Bulk Density 0.0190 g/cc
0.000686 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene  (discontinued **)
Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T..