Physical Properties Metric English Comments
Apparent Bulk Density 0.0800 g/cc
0.00289 lb/in³
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Apparent Bulk Density 0.0800 - 0.0900 g/cc
0.00289 - 0.00325 lb/in³
ISO 60
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Apparent Bulk Density 0.0800 g/cc
0.00289 lb/in³
Free-rise Density, Bayer test
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Apparent Bulk Density 0.0800 g/cc
0.00289 lb/in³
Free-rise Density, Bayer test
Covestro Bayfill® EA 6005 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Apparent Bulk Density 0.0800 - 1.15 g/cc
0.00289 - 0.0415 lb/in³
Average value: 0.818 g/cc Grade Count:16
Overview of materials for Epoxy, Molded, Glass Fiber Filler