Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.360 - 0.420 g/cc | 0.0130 - 0.0152 lb/in³ | |
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.360 - 0.950 g/cc | 0.0130 - 0.0343 lb/in³ | Average value: 0.665 g/cc Grade Count:26 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Apparent Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |