Physical Properties Metric English Comments
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
Geon® 1169
PolyOne Geon™ 140 Series 140X466 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
Geon® 1169
PolyOne Geon™ 140 Series 140X497 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
Tap density
Momentive Performance Materials HCP Boron Nitride (BN) Powder
Grade HCP is a fine mesh hexagonal Boron Nitride (BN) powder (99%, -325 mesh). It exhibits the unique properties of boron nitride in a form readily used in the production of many advanced materials..
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D792
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 25 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
Tap density
Carborundum CarboTherm™ CTL40 Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..
Apparent Bulk Density 0.400 - 0.500 g/cc
0.0145 - 0.0181 lb/in³
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group