Polymer Property : Apparent Bulk Density = 0.0164 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.455 g/cc
0.0164 lb/in³
MSZ ISO 60
BorsodChem ONGRO CPE 3602 N Chlorinated Polyethylene
IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r..