Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.526 g/cc | 0.0190 lb/in³ | ASTM D1895 |
Chevron Phillips 4538B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso.. |
|||
Apparent Bulk Density | 0.526 g/cc | 0.0190 lb/in³ | ASTM D1895 |
Chevron Phillips 5102 LDPE Injection Blow Molding Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Core Pin Release, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on GlossApplications:Squeeze Bottles, Perso.. |
|||
Apparent Bulk Density | 0.526 g/cc | 0.0190 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 4538A LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Apparent Bulk Density | 0.526 g/cc | 0.0190 lb/in³ | ASTM D1895 |
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Apparent Bulk Density | 0.526 g/cc | 0.0190 lb/in³ | Average value: 0.526 g/cc Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |