Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.545 - 0.577 g/cc | 0.0197 - 0.0208 lb/in³ | Average value: 0.569 g/cc Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Apparent Bulk Density | 0.449 - 0.577 g/cc | 0.0162 - 0.0208 lb/in³ | Average value: 0.534 g/cc Grade Count:9 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |