Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Apparent Bulk Density = 0.0260 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
DIN 53 466
3M Dyneon™ 1502 PTFE Powder  (discontinued **)
Type VI PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Apparent density per ASTM D1895
Plenco 4100 Phenolic, Granular, Compression Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Apparent density per ASTM D1895
Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D1895
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
TRM-37
Tipco Tipcolite® TG 613 Phenolic Compound, Mineral & Wood Flour, Soft Flow & Good Surface Finish
Soft Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: General PurposeProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India...
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
TRM-37
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
TRM-37
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties
Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie..
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved