Physical Properties Metric English Comments
Apparent Bulk Density 0.740 - 0.840 g/cc
0.0267 - 0.0303 lb/in³
IS 867-1963
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Apparent Bulk Density 0.750 - 0.840 g/cc
0.0271 - 0.0303 lb/in³
IS 867-1963
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..