Physical Properties Metric English Comments
Apparent Bulk Density 3.12 g/cc
0.113 lb/in³
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated
SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..
Apparent Bulk Density 3.12 g/cc
0.113 lb/in³
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Apparent Bulk Density 3.13 g/cc
0.113 lb/in³
Poco Graphite SUPERSiC® Basic Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..