Polymer Property : Apparent Bulk Density = 0.320 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.320 g/cc
0.0116 lb/in³
ASTM D792
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..