Apparent Bulk Density 1.75 g/cc
0.0632 lb/in³
Carlisle 201HD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Apparent Bulk Density 1.75 g/cc
0.0632 lb/in³
Carlisle 201LD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..