Physical Properties | Metric | English | Comments |
---|---|---|---|
Pore Size | 0.00500 microns | 0.000197 mil | Average Diameter |
NanoScale NanoActive® Magnesium Oxide NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperature.. |
|||
Pore Size | 0.00500 microns | 0.000197 mil | Median Pierce adsorption mesopore, based on surface area |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Pore Size | 0.00500 microns | 0.000197 mil | Median Pierce adsorption mesopore, based on surface area |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |