Polymer Property : Pore Size = 0.300 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Pore Size 0.300 microns
0.0118 mil
Poco Graphite ZXF-5Q Industrial Grade Graphite
SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..