Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Induction Time (OIT) | 10.0 - 118 min | 10.0 - 118 min | Average value: 70.8 min Grade Count:4 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Oxidative Induction Time (OIT) | 10.0 - 200 min | 10.0 - 200 min | Average value: 62.5 min Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Oxidative Induction Time (OIT) | 10.0 - 40.0 min | 10.0 - 40.0 min | Average value: 22.3 min Grade Count:23 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Oxidative Induction Time (OIT) | >= 10.0 min @Temperature 200 - 200 °C |
>= 10.0 min @Temperature 392 - 392 °F |
Average value: 10.0 min Grade Count:1 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |