Polymer Property : Oxidative Induction Time (OIT) = 20.0 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) 20.0 - 20.0 min

@Temperature 210 - 210 °C
20.0 - 20.0 min

@Temperature 410 - 410 °F
Average value: 20.0 min Grade Count:2
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..