Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco 220R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco 46 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Canopus® 46 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Capella® P 68 Texaco Capella P 68 delivers value through:Reduced oil carryover — Low volatility and greater ammonia immiscibility result in significantly less oil reaching the evaporator, increasing refrigeratio.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco ISO 46 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco ISO 68 Ammonia Refrigeration Oil FeaturesChevron Ammonia Refrigeration Oil provides superior wear protection for reciprocating, vane, and screw compressors.Chevron Ammonia Refrigeration Oil, formulated with ISOSYN® base stocks, is.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco ParaLux® 2401R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco ParaLux™ 2401 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco ParaMount™ 2401 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Rando® HD 68 Ashless Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Rykon® ISO 46 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Clarity® ISO 68 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |
|||
API Gravity | 31.8 ° | 31.8 ° | |
ChevronTexaco Rando® HD 46 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |