Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 122 SUS | 122 SUS | |
ChevronTexaco Elite-Cut® NL Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Saybolt Viscosity at 100°F | 122 SUS | 122 SUS | |
ChevronTexaco ISO 22 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Saybolt Viscosity at 100°F | 122 SUS | 122 SUS | |
ChevronTexaco Alcaid® 19 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |