Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1380 SUS
1380 SUS
ChevronTexaco 260 Compressor Oil
Chevron Compressor Oil 260 is a high viscosity index lubricant for use in natural gas compressors.It is formulated from a carefully selected blend of base oils and additives that provide protection ..