Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 560 SUS | 560 SUS | |
ChevronTexaco Tool Joint Compound FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads.It contains copper flake and graphite, forti.. |