Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 86 SUS
86 SUS
ChevronTexaco 8-T White Oil
FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma..
Saybolt Viscosity at 100°F 86 SUS
86 SUS
ChevronTexaco Packers Oil