Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 973 SUS | 973 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® AA Cooker & Valve Oil, High Temperature Water Resistant Food Grade ISO 220 Description: ANDEROL PQ AA Cooker & Valve Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Cooker &.. |