Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 105 SUS | 105 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 783-2 Series Synthetic Food Grade Greases, NLGI Grade 2 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |