Saybolt Viscosity at 210°F 191 SUS
191 SUS
ChevronTexaco ISO 680 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
Saybolt Viscosity at 210°F 191 SUS
191 SUS
ChevronTexaco Vanguard® 680
Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p..