Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 73.2 SUS | 73.2 SUS | ASTM D445 |
ChevronTexaco Cetus® PAO 100 Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie.. |