Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 81.3 SUS | 81.3 SUS | |
ChevronTexaco FM Seamer Oil FeaturesChevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications... |