Physical Properties Metric English Comments
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 21MB777 OPP Film
Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25ICT OPP Film
Product Description: A one-side sealable, very broad seal range coextruded BOPP. This film is designed for use in unsupported plain or surface printed high-speed horizontal applications. The enhance..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB400 OPP Film
Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB666 OPP Film
Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low seal temperature (VLTS) coating. VLTS coating provides excellent perf..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB866 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MBT666 OPP Film
Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 26MB600 OPP Film
Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 36MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa ..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 38MO447 OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 38MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 40MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 30MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW747 OPP Film
Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 35HM247 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial..
Water Vapor Transmission 1.10 g/m²/day

@Temperature 23.0 °C
0.0710 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 40MW647 OPP Film
Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & ..