Water Vapor Transmission 1.20 g/m²/day

@Temperature 38.0 °C
0.0770 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Metallyte™ 30MM680 OPP Film
Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS ..