Physical Properties Metric English Comments
Water Vapor Transmission 6.05 g/m²/day

@Temperature 38.0 °C
0.390 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 35MW647 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & ..
Water Vapor Transmission 6.05 g/m²/day

@Temperature 38.0 °C
0.390 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 33MW247 OPP Film