Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 15MB440 OPP Film
Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin ..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 19MB440 OPP Film
Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB080 OPP Film
Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB400 OPP Film
Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB666 OPP Film
Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB668 OPP Film
Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 21MB621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 21MBT621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel..
Water Vapor Transmission 6.98 g/m²/day

@Temperature 38.0 °C
0.450 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MBT666 OPP Film
Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as..