Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.060 g/10 min | 0.060 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont DGDP-2485 High Density Polyethylene Resin Pétromont® DGDP-2485 Natural is a high density polyethylene copolymer produced using the UNIPOL® process technology. DGDP-2485 is a high performance resin with very high melt strength, excellent .. |
|||
Melt Flow | 0.060 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.060 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Global GA-3750 High Density Polyethylene, Film Extrusion Grade Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsMeets FDA requirements as listed in food additives regulations 21 C.. |
|||
Melt Flow | 0.060 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.060 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l.. |
|||
Melt Flow | 0.060 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.060 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |