Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±8% |
Kazanorgsintez 102-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±8% |
Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±12% |
Kazanorgsintez 102-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±12% |
Kazanorgsintez 102-12K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min | 0.21 - 0.39 g/10 min | ±8% Superior Quality, ±12% Premium Quality |
Kazanorgsintez 153-02 K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±8% |
Kazanorgsintez 153-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±8% |
Kazanorgsintez 153-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min | 0.21 - 0.39 g/10 min | ±8% Superior Quality, ±12% Premium Quality |
Kazanorgsintez 153-10K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±12% |
Kazanorgsintez 153-12K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Melt Flow | 0.21 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.21 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |
|||
Melt Flow | 0.21 - 0.39 g/10 min @Load 21.6 kg |
0.21 - 0.39 g/10 min @Load 47.6 lb |
±12% |
Kazanorgsintez 153-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |