Polymer Property : Melt Flow = 0.24 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.24 - 0.36 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.24 - 0.36 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GF 5250 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 0.24 - 0.36 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.24 - 0.36 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem MB 0310 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Melt Flow 0.24 - 0.42 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.24 - 0.42 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GM 9450 F HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 0.24 g/10 min
0.24 g/10 min
JIS K7210
Stellarchem AB870LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..