Melt Flow 0.26 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet  (discontinued **)
Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str..
Melt Flow 0.26 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 g/10 min

@Load 4.76 lb,
Temperature 374 °F
LyondellBasell Lupolen® 3822 D GB 00350 MDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melt Flow 0.26 - 0.42 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 - 0.42 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GF 4950 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 0.26 - 0.42 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 - 0.42 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GF 4960 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 0.26 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.26 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound
Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds..