Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.66 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.66 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1003 VL 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Melt Flow | 0.66 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.66 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma.. |
|||
Melt Flow | 0.66 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.66 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1005 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for strength films, sealable at low temperature with some hot tack. Examples: rigid bags, deep-freeze packaging, laminates, co.. |
|||
Melt Flow | 0.66 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.66 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1005 VL 2C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for thermal agricultural films to 180 at 200 µ with diffusing effect, for greenhouse coverage.ISO d.. |
|||
Melt Flow | 0.66 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.66 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1006 VL 2E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 200 at 210 µm for greenhouse coverage.ISO data provided by the.. |