Polymer Property : Melt Flow = 1.25 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP640G Sheet and Thermoforming Grade Polypropylene
Moplen HP640G is the polypropylene Homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640G is a homopolymer particularly suitable for sheet and thermof..
Melt Flow 1.25 g/10 min
1.25 g/10 min
ExxonMobil Method
ExxonMobil Exceed™ 1318CA Blown Film Resin  (discontinued **)
Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi..
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene
Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor..
Melt Flow 1.25 g/10 min
1.25 g/10 min
ASTM D1238
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer  (discontinued **)
Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177..
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis FG5199 Linear Low Density Polyethylene
FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit..
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Westlake EF418 Low Density Polyethylene
WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera..
Melt Flow 1.25 g/10 min
1.25 g/10 min
ExxonMobil Method
ExxonMobil LD 334.57 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Melt Flow 1.25 g/10 min
1.25 g/10 min
ExxonMobil Method
ExxonMobil LD 334.82 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical