Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.37 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.37 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |