Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.572 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.572 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Melt Flow | 1.572 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.572 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Polystyrol 168 N GR 21 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |