Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.36 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.36 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |