Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.11 g/10 min | 11.11 g/10 min | ISO 1133 |
Styrolution Styrolux® 684 D SBC Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part.. |